Chemical Composition (%)
| C | Mn | Si | P | S | Ni | Cr | Mo | |
| Test | 0.12 | 0.38 | 0.18 | 0.002 | 0.014 | 0.083 | 0.035 | 0.005 |
Melting metal mechanical performance
| Tensile strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation ratio (%) | AKV(-30℃) | |||||||
| Test | 496 | 405 | 29 | 50 | ||||||
Reference Current(AC, DC-)
| Diameter | 3.2mm | 4.0mm | 5.0mm |
| Amperage | 60~80 | 90~110 | 140~160 |
Precautions:
- No baking is required.
- Impurities such as rust, oil stain and moisture must be cleared off the work piece before welding.
- While welding, the operating current should not be too large, and the welding electrode should not swing greatly.
Welding position: OH, F, H, HF, VD, VU