Chemical Composition of Deposited metal (%):
| C | Mn | Si | P | S | |
| Range | ≤0.18 | ≤2.00 | ≤0.90 | ≤0.030 | ≤0.030 |
| Test | 0.08 | 1.30 | 0.65 | 0.015 | 0.007 |
Mechanical properties of deposited metal:
| Tensile strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation ratio (%) | AKV(-20℃) | Shielding gas | |||||||
| Range | 490-670 | ≥390 | ≥18 | ≥27 | CO2 (purity≥99.8%) | ||||||
| Test | 545 | 450 | 26 | 105 | |||||||
Diffusion hydrogen content of deposited metal (Measured value): ≤10ml/100g
Reference Current (DC+)
| Diameter | 1.0mm | 1.2mm | 1.4mm | 1.6mm |
| Amperage | 100~170 | 180~280 | 200~280 | 240~300 |
Precautions:
- The work piece shall be degreased and derusted before welding.
- When welding, the gas flow rate is generally 20~25L/min
- the dry extension lengh of the wire should be 15~25mm while the wire welding.