Chemical Composition of Deposited metal (%):
| C | Mn | Si | P | S | Ni | Cr | Mo | V | Al | |
| Range | ≤0.30 | ≤1.75 | ≤0.60 | ≤0.03 | ≤0.03 | ≤0.50 | ≤0.20 | ≤0.30 | ≤0.08 | ≤1.8 |
| Test | 0.18 | 1.00 | 0.36 | 0.012 | 0.007 | 0.15 | 0.02 | 0.02 | 0.01 | 1.20 |
Mechanical properties of deposited metal:
| Tensile strength Rm (Mpa) | Elongation ratio (%) | |||||
| ≥490 | ≥18 | |||||
| Test | 570 | 25 | ||||
Shielding gas: NO
Reference Current (DC-)
| Diameter | 0.8mm | 0.9mm | 1.0mm |
| Welding current (A) | 60~130 | 60~150 | 60~150 |
| Welding voltage (V) | 14~21 | 15~22 | 15~22 |
Precautions:
- The work piece shall be degreased and derusted before welding.
- the dry extension lengh of the wire should be 10~15mm while the wire welding.